General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 255 [-] Show Material materials with Dureza Brinell of 255 [-] | |
Dureza Rockwell C | 23.0 °C | 25 [-] Show Material materials with Dureza Rockwell C of 25 [-] | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.95 - 1.2 % Show Material materials with Carbono of 0.95 - 1.2 % |
Cromo | 16 - 18 % Show Material materials with Cromo of 16 - 18 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 0.4 - 0.8 % Show Material materials with Molibdeno of 0.4 - 0.8 % |
Oxígeno | 2E-3 % Show Material materials with Oxígeno of 2E-3 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |