General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 201 [-] Show Material materials with Dureza Brinell of 201 [-] | |
Elongación A50 | 23.0 °C | 15 % Show Material materials with Elongación A50 of 15 % | |
Elongation A200 | 23.0 °C | 13 % Show Material materials with Elongation A200 of 13 % | |
Límite elástico | 23.0 °C | 550 MPa Show Material materials with Límite elástico of 550 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 655 MPa Show Material materials with Resistencia a la tracción of 655 MPa |
Chemical properties
Property | Value |
---|---|
Molibdeno | 0.01 - 0.3 % Show Material materials with Molibdeno of 0.01 - 0.3 % |
Niobio | 0.01 - 0.07 % Show Material materials with Niobio of 0.01 - 0.07 % |
Titanio | 0.03 % Show Material materials with Titanio of 0.03 % |
Vanadio | 0.02 - 0.2 % Show Material materials with Vanadio of 0.02 - 0.2 % |