General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Nickel Molybdenum Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Molybdenum Steel |
Elongación A50 | 20.0 °C | 0 - 17 % Show Material materials with Elongación A50 of 0 - 17 % | |
Estricción | 20.0 °C | 0 - 35 % Show Material materials with Estricción of 0 - 35 % | |
Resistencia a la tracción | 20.0 °C | 0 - 725 MPa Show Material materials with Resistencia a la tracción of 0 - 725 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 0 - 585 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 585 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K | Typical for Nickel Molybdenum Steel 20-300°C |
Temperatura de fusión | 1529 °C Show Material materials with Temperatura de fusión of 1529 °C | Typical for Nickel Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0 - 0.035 % Show Material materials with Azufre of 0 - 0.035 % |
Carbono | 0.05 - 0.2 % Show Material materials with Carbono of 0.05 - 0.2 % |
Cobre | 0 - 0.5 % Show Material materials with Cobre of 0 - 0.5 % |
Fósforo | 0 - 0.04 % Show Material materials with Fósforo of 0 - 0.04 % |
Manganeso | 0.5 - 0.8 % Show Material materials with Manganeso of 0.5 - 0.8 % |
Molibdeno | 0.45 - 0.65 % Show Material materials with Molibdeno of 0.45 - 0.65 % |
Silicona | 0 - 0.6 % Show Material materials with Silicona of 0 - 0.6 % |
Vanadio | 0 - 0.03 % Show Material materials with Vanadio of 0 - 0.03 % |
Wolframio | 0 - 0.1 % Show Material materials with Wolframio of 0 - 0.1 % |