General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación A50 | 23.0 °C | 17 % Show Material materials with Elongación A50 of 17 % | |
Elongation A200 | 23.0 °C | 13 % Show Material materials with Elongation A200 of 13 % | |
Límite elástico Rp0.5 | 23.0 °C | 305 MPa Show Material materials with Límite elástico Rp0.5 of 305 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 550 MPa Show Material materials with Resistencia a la tracción of 550 MPa |