General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 183 - 271 [-] Show Material materials with Dureza Brinell of 183 - 271 [-] | |
Dureza Rockwell B | 23.0 °C | 88 [-] Show Material materials with Dureza Rockwell B of 88 [-] | |
Dureza Rockwell C | 23.0 °C | 25 [-] Show Material materials with Dureza Rockwell C of 25 [-] | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cromo | 16 - 18 % Show Material materials with Cromo of 16 - 18 % |
Fósforo | 0.06 % Show Material materials with Fósforo of 0.06 % |
Manganeso | 7 - 9 % Show Material materials with Manganeso of 7 - 9 % |
Nitrógeno | 0.08 - 0.18 % Show Material materials with Nitrógeno of 0.08 - 0.18 % |
Níquel | 8 - 9 % Show Material materials with Níquel of 8 - 9 % |
Silicona | 3.5 - 4.5 % Show Material materials with Silicona of 3.5 - 4.5 % |