General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.6 - 7.8 g/cm³ Show Material materials with Densidad of 7.6 - 7.8 g/cm³ | Typical for Ferritic Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Ferritic Stainless Steel |
Dureza Brinell | 23.0 °C | 207 [-] Show Material materials with Dureza Brinell of 207 [-] | |
Dureza Rockwell B | 23.0 °C | 95 [-] Show Material materials with Dureza Rockwell B of 95 [-] | |
Elongación A50 | 23.0 °C | 20 % Show Material materials with Elongación A50 of 20 % | |
Límite elástico Rp 0,2 | 23.0 °C | 380 MPa Show Material materials with Límite elástico Rp 0,2 of 380 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Ferritic Stainless Steel |
Módulo elástico | 23.0 °C | 220 GPa Show Material materials with Módulo elástico of 220 GPa | Typical for Ferritic Stainless Steel |
Resistencia a la tracción | 23.0 °C | 485 MPa Show Material materials with Resistencia a la tracción of 485 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 420 - 586 J/(kg·K) Show Material materials with Calor específico of 420 - 586 J/(kg·K) | Typical for Ferritic Stainless Steel |
Coeficiente de dilatación térmica | 23.0 °C | 9.3E-6 - 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 9.3E-6 - 1.2E-5 1/K | Typical for Ferritic Stainless Steel |
Conductividad térmica | 23.0 °C | 11 - 22 W/(m·K) Show Material materials with Conductividad térmica of 11 - 22 W/(m·K) | Typical for Ferritic Stainless Steel |
Temperatura de fusión | 1425 - 1530 °C Show Material materials with Temperatura de fusión of 1425 - 1530 °C | Typical for Ferritic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 6E-7 - 7.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 - 7.5E-7 Ω·m | Typical for Ferritic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.01 % Show Material materials with Carbono of 0.01 % |
Cobre | 0.15 % Show Material materials with Cobre of 0.15 % |
Cromo | 28 - 30 % Show Material materials with Cromo of 28 - 30 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.3 % Show Material materials with Manganeso of 0.3 % |
Molibdeno | 3.5 - 4.2 % Show Material materials with Molibdeno of 3.5 - 4.2 % |
Nitrógeno | 0.02 % Show Material materials with Nitrógeno of 0.02 % |
Níquel | 2 - 2.5 % Show Material materials with Níquel of 2 - 2.5 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |