General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Duplex Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Duplex Stainless Steel |
Elongación A50 | 20.0 °C | 20 % Show Material materials with Elongación A50 of 20 % | |
Módulo elástico | 20.0 °C | 200 GPa Show Material materials with Módulo elástico of 200 GPa | Typical for Duplex Stainless Steel |
Resistencia a la tracción | 20.0 °C | 455 MPa Show Material materials with Resistencia a la tracción of 455 MPa | |
Yield Strength Rp0.2, short transverse | 20.0 °C | 360 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 360 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 440 - 502 J/(kg·K) Show Material materials with Calor específico of 440 - 502 J/(kg·K) | Typical for Duplex Stainless Steel |
Coeficiente de dilatación térmica | 20.0 °C | 1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 1/K | Typical for Duplex Stainless Steel |
Conductividad térmica | 20.0 °C | 13 - 30 W/(m·K) Show Material materials with Conductividad térmica of 13 - 30 W/(m·K) | Typical for Duplex Stainless Steel |
Temperatura de fusión | 1375 - 1450 °C Show Material materials with Temperatura de fusión of 1375 - 1450 °C | Typical for Duplex Stainless Steel | |
Temperatura máx. de funcionamiento | 300 °C Show Material materials with Temperatura máx. de funcionamiento of 300 °C | Typical for Duplex Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.3 % Show Material materials with Carbono of 0.3 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 1.6 % Show Material materials with Manganeso of 1.6 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |