General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Manganese Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Manganese Steel |
Dureza Brinell | 23.0 °C | 248 - 327 [-] Show Material materials with Dureza Brinell of 248 - 327 [-] | |
Dureza Rockwell C | 23.0 °C | 24 - 35 [-] Show Material materials with Dureza Rockwell C of 24 - 35 [-] | |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Manganese Steel |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 510 - 553 J/(kg·K) Show Material materials with Calor específico of 510 - 553 J/(kg·K) | Typical for Manganese Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.33E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.33E-5 1/K | Typical for Manganese Steel |
Conductividad térmica | 23.0 °C | 14 - 16 W/(m·K) Show Material materials with Conductividad térmica of 14 - 16 W/(m·K) | Typical for Manganese Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Manganese Steel |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.15 % Show Material materials with Aluminio of 0.15 % |
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Carbono | 0.36 - 0.47 % Show Material materials with Carbono of 0.36 - 0.47 % |
Cromo | 0.8 - 1.15 % Show Material materials with Cromo of 0.8 - 1.15 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 0.45 - 0.7 % Show Material materials with Manganeso of 0.45 - 0.7 % |
Molibdeno | 0.5 - 0.65 % Show Material materials with Molibdeno of 0.5 - 0.65 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |
Vanadio | 0.25 - 0.35 % Show Material materials with Vanadio of 0.25 - 0.35 % |