General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 20.0 °C | 95 [-] Show Material materials with Dureza Brinell of 95 [-] | |
Dureza Vickers | 20.0 °C | 225 [-] Show Material materials with Dureza Vickers of 225 [-] | |
Elongación A80 | 20.0 °C | 13 % Show Material materials with Elongación A80 of 13 % | |
Límite elástico Rp 0,2 | 20.0 °C | 580 MPa Show Material materials with Límite elástico Rp 0,2 of 580 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 20.0 °C | 720 MPa Show Material materials with Resistencia a la tracción of 720 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.45 - 0.52 % Show Material materials with Carbono of 0.45 - 0.52 % |
Cromo | 0.4 % Show Material materials with Cromo of 0.4 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.5 - 0.8 % Show Material materials with Manganeso of 0.5 - 0.8 % |
Molibdeno | 0.1 % Show Material materials with Molibdeno of 0.1 % |
Níquel | 0.4 % Show Material materials with Níquel of 0.4 % |
Silicona | 1.6 - 2 % Show Material materials with Silicona of 1.6 - 2 % |