General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.7 - 8.7 g/cm³ Show Material materials with Densidad of 7.7 - 8.7 g/cm³ | Typical for Leaded Phosphor Bronze |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Elongación | 23.0 °C | 15 % Show Material materials with Elongación of 15 % | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Resistencia a la tracción | 23.0 °C | 637 MPa Show Material materials with Resistencia a la tracción of 637 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 380 J/(kg·K) Show Material materials with Calor específico of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Aluminio | 8.5 - 10.5 % Show Material materials with Aluminio of 8.5 - 10.5 % |
Cobre | 77 - 84 % Show Material materials with Cobre of 77 - 84 % |
Hierro | 3.5 - 6 % Show Material materials with Hierro of 3.5 - 6 % |
Manganeso | 0.5 - 2 % Show Material materials with Manganeso of 0.5 - 2 % |
Níquel | 4 - 6 % Show Material materials with Níquel of 4 - 6 % |