General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.6 - 7.77 g/cm³ Show Material materials with Densidad of 7.6 - 7.77 g/cm³ | Typical for White Cast Iron |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.27 [-] Show Material materials with Coeficiente de Poisson of 0.27 [-] | Typical for Cast Iron |
Dureza Vickers | 20.0 °C | 350 [-] Show Material materials with Dureza Vickers of 350 [-] | |
Módulo de cizallamiento | 23.0 °C | 41 GPa Show Material materials with Módulo de cizallamiento of 41 GPa | Typical for Cast Iron |
Módulo elástico | 23.0 °C | 165 - 240 GPa Show Material materials with Módulo elástico of 165 - 240 GPa | Typical for White Cast Iron |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | Typical for White Cast Iron |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 1/K | Typical for White Cast Iron |
Conductividad térmica | 23.0 °C | 22 - 30 W/(m·K) Show Material materials with Conductividad térmica of 22 - 30 W/(m·K) | Typical for White Cast Iron |
Temperatura de fusión | 1209 °C Show Material materials with Temperatura de fusión of 1209 °C | Typical for White Cast Iron |
Chemical properties
Property | Value |
---|---|
Carbono | 2.4 - 3.9 % Show Material materials with Carbono of 2.4 - 3.9 % |
Cromo | 2 % Show Material materials with Cromo of 2 % |
Manganeso | 0.2 - 1 % Show Material materials with Manganeso of 0.2 - 1 % |
Silicona | 0.4 - 1.5 % Show Material materials with Silicona of 0.4 - 1.5 % |