General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel | |||
Elongación | 10.1 % Show Material materials with Elongación of 10.1 % | Predicted Value, A200 | |||
16.2 % Show Material materials with Elongación of 16.2 % | Predicted Value, A80 | ||||
19 % Show Material materials with Elongación of 19 % | Quenched and Tempered | ASTM A709 | Plate, Bar | A50 | |
19.6 % Show Material materials with Elongación of 19.6 % | Predicted Value, A80 Transverse | ||||
20.5 % Show Material materials with Elongación of 20.5 % | Predicted Value, Transverse | ||||
22.8 % Show Material materials with Elongación of 22.8 % | Predicted Value | ||||
Estricción | 42.9 % Show Material materials with Estricción of 42.9 % | Predicted Value, Transverse | |||
45.7 % Show Material materials with Estricción of 45.7 % | Predicted Value | ||||
Módulo de cizallamiento | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | Typical for Low Carbon Steel | |||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Low Carbon Steel | |||
Resistencia a la tracción | 585 - 760 MPa Show Material materials with Resistencia a la tracción of 585 - 760 MPa | Quenched and Tempered | ASTM A709 | Plate, Bar | |
Resistencia al cizallamiento | 644.8 MPa Show Material materials with Resistencia al cizallamiento of 644.8 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 465 J/(kg·K) Show Material materials with Calor específico of 465 J/(kg·K) | Typical for Low Carbon Steel |
Coeficiente de dilatación térmica | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Conductividad térmica | 25 - 93 W/(m·K) Show Material materials with Conductividad térmica of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel |
Temperatura máx. de funcionamiento | 326.5 °C Show Material materials with Temperatura máx. de funcionamiento of 326.5 °C | Predicted Value, Long |
500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 8 S/m Show Material materials with Conductividad eléctrica of 8 S/m | Predicted Value |
Resistividad eléctrica | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |