Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 17 - 20 % Show Material materials with Elongación A50 of 17 - 20 % |
Elongation A200 | 23.0 °C | 14 % Show Material materials with Elongation A200 of 14 % |
Límite elástico | 23.0 °C | 240 MPa Show Material materials with Límite elástico of 240 MPa |
Resistencia a la tracción | 23.0 °C | 415 - 515 MPa Show Material materials with Resistencia a la tracción of 415 - 515 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 - 0.08 % Show Material materials with Aluminio of 0.02 - 0.08 % |
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Carbono | 0.25 % Show Material materials with Carbono of 0.25 % |
Cobre | 0.4 % Show Material materials with Cobre of 0.4 % |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1.2 % Show Material materials with Manganeso of 1.2 % |
Molibdeno | 0.12 % Show Material materials with Molibdeno of 0.12 % |
Niobio | 0.02 % Show Material materials with Niobio of 0.02 % |
Níquel | 0.4 % Show Material materials with Níquel of 0.4 % |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |
Titanio | 0.03 % Show Material materials with Titanio of 0.03 % |