Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 0 - 20 % Show Material materials with Elongación A50 of 0 - 20 % |
Energía de impacto Charpy | 20.0 °C | 0 - 27 J Show Material materials with Energía de impacto Charpy of 0 - 27 J |
Resistencia a la tracción | 20.0 °C | 0 - 620 MPa Show Material materials with Resistencia a la tracción of 0 - 620 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 0 - 585 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 0 - 585 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0 - 0.025 % Show Material materials with Azufre of 0 - 0.025 % |
Carbono | 0 - 0.07 % Show Material materials with Carbono of 0 - 0.07 % |
Cobre | 1 - 1.3 % Show Material materials with Cobre of 1 - 1.3 % |
Cromo | 0.6 - 0.9 % Show Material materials with Cromo of 0.6 - 0.9 % |
Fósforo | 0 - 0.03 % Show Material materials with Fósforo of 0 - 0.03 % |
Manganeso | 0.4 - 0.7 % Show Material materials with Manganeso of 0.4 - 0.7 % |
Molibdeno | 0.15 - 0.25 % Show Material materials with Molibdeno of 0.15 - 0.25 % |
Niobio | 0 - 0.02 % Show Material materials with Niobio of 0 - 0.02 % |
Níquel | 0.7 - 1 % Show Material materials with Níquel of 0.7 - 1 % |
Silicona | 0 - 0.4 % Show Material materials with Silicona of 0 - 0.4 % |