Mecánica
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Carbono | 0.07 % Show Material materials with Carbono of 0.07 % |
Cobre | 3 - 4 % Show Material materials with Cobre of 3 - 4 % |
Cromo | 19 - 22 % Show Material materials with Cromo of 19 - 22 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Molibdeno | 2 - 3 % Show Material materials with Molibdeno of 2 - 3 % |
Níquel | 27.5 - 30.5 % Show Material materials with Níquel of 27.5 - 30.5 % |
Silicona | 1.5 % Show Material materials with Silicona of 1.5 % |