Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 217 [-] Show Material materials with Dureza Brinell of 217 [-] |
Dureza Rockwell B | 20.0 °C | 95 [-] Show Material materials with Dureza Rockwell B of 95 [-] |
Elongación A50 | 20.0 °C | 30 % Show Material materials with Elongación A50 of 30 % |
Resistencia a la tracción | 20.0 °C | 550 MPa Show Material materials with Resistencia a la tracción of 550 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 240 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 240 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Carbono | 0.07 % Show Material materials with Carbono of 0.07 % |
Cobre | 3 - 4 % Show Material materials with Cobre of 3 - 4 % |
Cromo | 19 - 21 % Show Material materials with Cromo of 19 - 21 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 2 - 3 % Show Material materials with Molibdeno of 2 - 3 % |
Níquel | 32 - 38 % Show Material materials with Níquel of 32 - 38 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |