General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 250 [-] Show Material materials with Dureza Brinell of 250 [-] | |
Elongación A50 | 23.0 °C | 40 % Show Material materials with Elongación A50 of 40 % | |
Límite elástico Rp 0,2 | 23.0 °C | 430 MPa Show Material materials with Límite elástico Rp 0,2 of 430 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 750 MPa Show Material materials with Resistencia a la tracción of 750 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 5E-3 % Show Material materials with Azufre of 5E-3 % |
Carbono | 0.02 % Show Material materials with Carbono of 0.02 % |
Cobre | 0.3 - 0.6 % Show Material materials with Cobre of 0.3 - 0.6 % |
Cromo | 24 - 25 % Show Material materials with Cromo of 24 - 25 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 2 - 4 % Show Material materials with Manganeso of 2 - 4 % |
Molibdeno | 7 - 8 % Show Material materials with Molibdeno of 7 - 8 % |
Nitrógeno | 0.45 - 0.55 % Show Material materials with Nitrógeno of 0.45 - 0.55 % |
Níquel | 21 - 23 % Show Material materials with Níquel of 21 - 23 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |