Mecánica
Chemical properties
Property | Value |
---|---|
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.35 % Show Material materials with Carbono of 0.35 % |
Cobre | 26 - 33 % Show Material materials with Cobre of 26 - 33 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 3.5 % Show Material materials with Hierro of 3.5 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Niobio | 0.5 % Show Material materials with Niobio of 0.5 % |
Silicona | 2 % Show Material materials with Silicona of 2 % |