Chemical properties
Property | Value |
---|---|
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.12 % Show Material materials with Carbono of 0.12 % |
Cromo | 15.5 - 17.5 % Show Material materials with Cromo of 15.5 - 17.5 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 4.5 - 7.5 % Show Material materials with Hierro of 4.5 - 7.5 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 16 - 18 % Show Material materials with Molibdeno of 16 - 18 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Vanadio | 0.2 - 0.4 % Show Material materials with Vanadio of 0.2 - 0.4 % |
Wolframio | 3.75 - 5.25 % Show Material materials with Wolframio of 3.75 - 5.25 % |