Chemical properties
Property | Value |
---|---|
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.07 % Show Material materials with Carbono of 0.07 % |
Cromo | 17 - 20 % Show Material materials with Cromo of 17 - 20 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 3 % Show Material materials with Hierro of 3 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 17 - 20 % Show Material materials with Molibdeno of 17 - 20 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |