General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.8 g/cm³ Show Material materials with Densidad of 8.8 g/cm³ | Typical for Nickel Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Steel |
Elongación A50 | 23.0 °C | 20 % Show Material materials with Elongación A50 of 20 % | |
Límite elástico | 23.0 °C | 275 MPa Show Material materials with Límite elástico of 275 MPa | |
Módulo de cizallamiento | 23.0 °C | 76 GPa Show Material materials with Módulo de cizallamiento of 76 GPa | Typical for Nickel Steel |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Nickel Steel |
Resistencia a la tracción | 23.0 °C | 495 MPa Show Material materials with Resistencia a la tracción of 495 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 456 J/(kg·K) Show Material materials with Calor específico of 456 J/(kg·K) | Typical for Nickel Steel |
Conductividad térmica | 23.0 °C | 10 - 50 W/(m·K) Show Material materials with Conductividad térmica of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Temperatura de fusión | 1316 - 1595 °C Show Material materials with Temperatura de fusión of 1316 - 1595 °C | Typical for Nickel Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.02 % Show Material materials with Carbono of 0.02 % |
Cromo | 15 - 17.5 % Show Material materials with Cromo of 15 - 17.5 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 2 % Show Material materials with Hierro of 2 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 15 - 17.5 % Show Material materials with Molibdeno of 15 - 17.5 % |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % |
Wolframio | 1 % Show Material materials with Wolframio of 1 % |