Mecánica
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.06 % Show Material materials with Carbono of 0.06 % |
Cromo | 20 - 23 % Show Material materials with Cromo of 20 - 23 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 5 % Show Material materials with Hierro of 5 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 8 - 10 % Show Material materials with Molibdeno of 8 - 10 % |
Niobio | 3.15 - 4.5 % Show Material materials with Niobio of 3.15 - 4.5 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |