General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 331 [-] Show Material materials with Dureza Brinell of 331 [-] | |
Dureza Rockwell C | 23.0 °C | 35 [-] Show Material materials with Dureza Rockwell C of 35 [-] | |
Elongación A50 | 23.0 °C | 10 % Show Material materials with Elongación A50 of 10 % | |
Estricción | 23.0 °C | 40 % Show Material materials with Estricción of 40 % | |
Límite elástico Rp 0,2 | 23.0 °C | 1035 MPa Show Material materials with Límite elástico Rp 0,2 of 1035 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 1170 MPa Show Material materials with Resistencia a la tracción of 1170 MPa |