General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 283 [-] Show Material materials with Dureza Brinell of 283 [-] | |
Dureza Rockwell C | 23.0 °C | 30 [-] Show Material materials with Dureza Rockwell C of 30 [-] | |
Elongación A50 | 23.0 °C | 14 % Show Material materials with Elongación A50 of 14 % | |
Elongación A50 transversal | 23.0 °C | 14 % Show Material materials with Elongación A50 transversal of 14 % | |
Estricción | 23.0 °C | 50 % Show Material materials with Estricción of 50 % | |
Hardness, Brinell, trans | 23.0 °C | 283 [-] Show Material materials with Hardness, Brinell, trans of 283 [-] | |
Límite elástico Rp 0,2 | 23.0 °C | 620 MPa Show Material materials with Límite elástico Rp 0,2 of 620 MPa | |
Límite elástico transversal Rp 0,2 | 23.0 °C | 620 MPa Show Material materials with Límite elástico transversal Rp 0,2 of 620 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Reducción de área, transversal | 23.0 °C | 50 % Show Material materials with Reducción de área, transversal of 50 % | |
Resistencia a la tracción | 23.0 °C | 930 MPa Show Material materials with Resistencia a la tracción of 930 MPa | |
Resistencia a la tracción transversal | 23.0 °C | 930 MPa Show Material materials with Resistencia a la tracción transversal of 930 MPa |