General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 444 [-] Show Material materials with Dureza Brinell of 444 [-] | |
Dureza Rockwell C | 23.0 °C | 47 [-] Show Material materials with Dureza Rockwell C of 47 [-] | |
Elongación A50 | 23.0 °C | 10 % Show Material materials with Elongación A50 of 10 % | |
Elongación A50 transversal | 23.0 °C | 8 % Show Material materials with Elongación A50 transversal of 8 % | |
Estricción | 23.0 °C | 45 % Show Material materials with Estricción of 45 % | |
Hardness, Brinell, trans | 23.0 °C | 444 [-] Show Material materials with Hardness, Brinell, trans of 444 [-] | |
Límite elástico Rp 0,2 | 23.0 °C | 1515 MPa Show Material materials with Límite elástico Rp 0,2 of 1515 MPa | |
Límite elástico transversal Rp 0,2 | 23.0 °C | 1515 MPa Show Material materials with Límite elástico transversal Rp 0,2 of 1515 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Reducción de área, transversal | 23.0 °C | 35 % Show Material materials with Reducción de área, transversal of 35 % | |
Resistencia a la tracción | 23.0 °C | 1655 MPa Show Material materials with Resistencia a la tracción of 1655 MPa | |
Resistencia a la tracción transversal | 23.0 °C | 1655 MPa Show Material materials with Resistencia a la tracción transversal of 1655 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.02 % Show Material materials with Carbono of 0.02 % |
Cromo | 11 - 12.5 % Show Material materials with Cromo of 11 - 12.5 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.25 % Show Material materials with Manganeso of 0.25 % |
Molibdeno | 0.75 - 1.25 % Show Material materials with Molibdeno of 0.75 - 1.25 % |
Níquel | 10.75 - 11.25 % Show Material materials with Níquel of 10.75 - 11.25 % |
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % |
Titanio | 1.5 - 1.8 % Show Material materials with Titanio of 1.5 - 1.8 % |