General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Rockwell B | 23.0 °C | 100 [-] Show Material materials with Dureza Rockwell B of 100 [-] | |
Elongación A50 | 23.0 °C | 25 % Show Material materials with Elongación A50 of 25 % | |
Límite elástico | 23.0 °C | 450 MPa Show Material materials with Límite elástico of 450 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 1035 MPa Show Material materials with Resistencia a la tracción of 1035 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.75 - 1.5 % Show Material materials with Aluminio of 0.75 - 1.5 % |
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.09 % Show Material materials with Carbono of 0.09 % |
Cromo | 14 - 16 % Show Material materials with Cromo of 14 - 16 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 2 - 3 % Show Material materials with Molibdeno of 2 - 3 % |
Níquel | 6.5 - 7.7 % Show Material materials with Níquel of 6.5 - 7.7 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |