General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Rockwell C | 23.0 °C | 30 [-] Show Material materials with Dureza Rockwell C of 30 [-] | |
Elongación A50 | 23.0 °C | 8 - 12 % Show Material materials with Elongación A50 of 8 - 12 % | |
Límite elástico | 23.0 °C | 585 - 620 MPa Show Material materials with Límite elástico of 585 - 620 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 1380 MPa Show Material materials with Resistencia a la tracción of 1380 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.07 - 0.11 % Show Material materials with Carbono of 0.07 - 0.11 % |
Cromo | 16 - 17 % Show Material materials with Cromo of 16 - 17 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 0.5 - 1.25 % Show Material materials with Manganeso of 0.5 - 1.25 % |
Molibdeno | 2.5 - 3.2 % Show Material materials with Molibdeno of 2.5 - 3.2 % |
Níquel | 4 - 5 % Show Material materials with Níquel of 4 - 5 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |