General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Duplex Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Duplex Stainless Steel |
Dureza Brinell | 23.0 °C | 300 [-] Show Material materials with Dureza Brinell of 300 [-] | |
Dureza Rockwell C | 23.0 °C | 32 [-] Show Material materials with Dureza Rockwell C of 32 [-] | |
Dureza Vickers | 23.0 °C | 300 [-] Show Material materials with Dureza Vickers of 300 [-] | |
Elongación A50 | 23.0 °C | 25 % Show Material materials with Elongación A50 of 25 % | |
Límite elástico | 23.0 °C | 550 - 650 MPa Show Material materials with Límite elástico of 550 - 650 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Duplex Stainless Steel |
Módulo elástico | 23.0 °C | 200 GPa Show Material materials with Módulo elástico of 200 GPa | Typical for Duplex Stainless Steel |
Resistencia a la tracción | 23.0 °C | 750 - 800 MPa Show Material materials with Resistencia a la tracción of 750 - 800 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 440 - 502 J/(kg·K) Show Material materials with Calor específico of 440 - 502 J/(kg·K) | Typical for Duplex Stainless Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 1/K | Typical for Duplex Stainless Steel |
Conductividad térmica | 23.0 °C | 13 - 30 W/(m·K) Show Material materials with Conductividad térmica of 13 - 30 W/(m·K) | Typical for Duplex Stainless Steel |
Temperatura de fusión | 1375 - 1450 °C Show Material materials with Temperatura de fusión of 1375 - 1450 °C | Typical for Duplex Stainless Steel | |
Temperatura máx. de funcionamiento | 300 °C Show Material materials with Temperatura máx. de funcionamiento of 300 °C | Typical for Duplex Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Cobre | 0.8 % Show Material materials with Cobre of 0.8 % |
Cromo | 28 - 30 % Show Material materials with Cromo of 28 - 30 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.8 - 1.5 % Show Material materials with Manganeso of 0.8 - 1.5 % |
Molibdeno | 1.5 - 2.6 % Show Material materials with Molibdeno of 1.5 - 2.6 % |
Nitrógeno | 0.3 - 0.4 % Show Material materials with Nitrógeno of 0.3 - 0.4 % |
Níquel | 5.8 - 7.5 % Show Material materials with Níquel of 5.8 - 7.5 % |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % |