General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación A50 | 23.0 °C | 25 - 35 % Show Material materials with Elongación A50 of 25 - 35 % | |
Límite elástico | 23.0 °C | 260 - 270 MPa Show Material materials with Límite elástico of 260 - 270 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 600 - 650 MPa Show Material materials with Resistencia a la tracción of 600 - 650 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.04 - 0.08 % Show Material materials with Carbono of 0.04 - 0.08 % |
Cerio | 0.03 - 0.08 % Show Material materials with Cerio of 0.03 - 0.08 % |
Cromo | 24 - 26 % Show Material materials with Cromo of 24 - 26 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Nitrógeno | 0.12 - 0.18 % Show Material materials with Nitrógeno of 0.12 - 0.18 % |
Níquel | 34 - 36 % Show Material materials with Níquel of 34 - 36 % |
Silicona | 1.2 - 2 % Show Material materials with Silicona of 1.2 - 2 % |