Mecánica
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.02 % Show Material materials with Carbono of 0.02 % |
Cobre | 0.5 - 1.5 % Show Material materials with Cobre of 0.5 - 1.5 % |
Cromo | 19 - 21 % Show Material materials with Cromo of 19 - 21 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 6 - 7 % Show Material materials with Molibdeno of 6 - 7 % |
Nitrógeno | 0.15 - 0.25 % Show Material materials with Nitrógeno of 0.15 - 0.25 % |
Níquel | 24 - 26 % Show Material materials with Níquel of 24 - 26 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |