Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 35 % Show Material materials with Elongación A50 of 35 % |
Resistencia a la tracción | 20.0 °C | 425 MPa Show Material materials with Resistencia a la tracción of 425 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 170 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 170 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Carbono | 0.07 % Show Material materials with Carbono of 0.07 % |
Cobre | 3 - 4 % Show Material materials with Cobre of 3 - 4 % |
Cromo | 19 - 22 % Show Material materials with Cromo of 19 - 22 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Molibdeno | 2 - 3 % Show Material materials with Molibdeno of 2 - 3 % |
Níquel | 27.5 - 30.5 % Show Material materials with Níquel of 27.5 - 30.5 % |
Silicona | 1.5 % Show Material materials with Silicona of 1.5 % |