Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 15 % Show Material materials with Elongación A50 of 15 % |
Resistencia a la tracción | 20.0 °C | 450 MPa Show Material materials with Resistencia a la tracción of 450 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 195 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 195 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.04 % Show Material materials with Azufre of 0.04 % |
Carbono | 0.25 - 0.35 % Show Material materials with Carbono of 0.25 - 0.35 % |
Cromo | 13 - 17 % Show Material materials with Cromo of 13 - 17 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 0.5 % Show Material materials with Molibdeno of 0.5 % |
Níquel | 33 - 37 % Show Material materials with Níquel of 33 - 37 % |
Silicona | 2.5 % Show Material materials with Silicona of 2.5 % |