General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación A50 | 23.0 °C | 18 - 28 % Show Material materials with Elongación A50 of 18 - 28 % | |
Energía de impacto Charpy | 23.0 °C | 17.6 J Show Material materials with Energía de impacto Charpy of 17.6 J | |
Límite elástico | 23.0 °C | 315 MPa Show Material materials with Límite elástico of 315 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 435 - 610 MPa Show Material materials with Resistencia a la tracción of 435 - 610 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % |
Cobre | 0.75 - 1.25 % Show Material materials with Cobre of 0.75 - 1.25 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.4 - 1.06 % Show Material materials with Manganeso of 0.4 - 1.06 % |
Níquel | 1.6 - 2.24 % Show Material materials with Níquel of 1.6 - 2.24 % |