General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación A50 | 23.0 °C | 20 - 30 % Show Material materials with Elongación A50 of 20 - 30 % | |
Energía de impacto Charpy | 23.0 °C | 17.6 J Show Material materials with Energía de impacto Charpy of 17.6 J | |
Límite elástico | 23.0 °C | 240 MPa Show Material materials with Límite elástico of 240 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 450 - 620 MPa Show Material materials with Resistencia a la tracción of 450 - 620 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.05 % Show Material materials with Azufre of 0.05 % |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Manganeso | 0.31 - 0.64 % Show Material materials with Manganeso of 0.31 - 0.64 % |
Níquel | 3.2 - 3.8 % Show Material materials with Níquel of 3.2 - 3.8 % |
Silicona | 0.13 - 0.37 % Show Material materials with Silicona of 0.13 - 0.37 % |