Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 20 % Show Material materials with Elongación A50 of 20 % |
Límite elástico Rp 0,2 | 23.0 °C | 275 MPa Show Material materials with Límite elástico Rp 0,2 of 275 MPa |
Resistencia a la tracción | 23.0 °C | 495 MPa Show Material materials with Resistencia a la tracción of 495 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.02 % Show Material materials with Carbono of 0.02 % |
Cromo | 15 - 17.5 % Show Material materials with Cromo of 15 - 17.5 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 2 % Show Material materials with Hierro of 2 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 15 - 17.5 % Show Material materials with Molibdeno of 15 - 17.5 % |
Silicona | 0.8 % Show Material materials with Silicona of 0.8 % |
Wolframio | 1 % Show Material materials with Wolframio of 1 % |