General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación A50 | 23.0 °C | 30 % Show Material materials with Elongación A50 of 30 % | |
Estricción | 23.0 °C | 50 % Show Material materials with Estricción of 50 % | |
Límite elástico Rp 0,2 | 23.0 °C | 205 MPa Show Material materials with Límite elástico Rp 0,2 of 205 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 550 MPa Show Material materials with Resistencia a la tracción of 550 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.1 - 0.2 % Show Material materials with Carbono of 0.1 - 0.2 % |
Cromo | 7 - 9 % Show Material materials with Cromo of 7 - 9 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 0.5 - 0.8 % Show Material materials with Manganeso of 0.5 - 0.8 % |
Níquel | 19 - 22 % Show Material materials with Níquel of 19 - 22 % |
Silicona | 1 - 1.4 % Show Material materials with Silicona of 1 - 1.4 % |