Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 30 % Show Material materials with Elongación A50 of 30 % |
Estricción | 20.0 °C | 50 % Show Material materials with Estricción of 50 % |
Resistencia a la tracción | 20.0 °C | 550 MPa Show Material materials with Resistencia a la tracción of 550 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 240 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 240 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.06 % Show Material materials with Carbono of 0.06 % |
Cromo | 20.5 - 23.5 % Show Material materials with Cromo of 20.5 - 23.5 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 4 - 6 % Show Material materials with Manganeso of 4 - 6 % |
Molibdeno | 1.5 - 3 % Show Material materials with Molibdeno of 1.5 - 3 % |
Niobio | 0.1 - 0.3 % Show Material materials with Niobio of 0.1 - 0.3 % |
Níquel | 11.5 - 13.5 % Show Material materials with Níquel of 11.5 - 13.5 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |