General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 248 [-] Show Material materials with Dureza Brinell of 248 [-] | |
Elongación A50 | 23.0 °C | 20 % Show Material materials with Elongación A50 of 20 % | |
Estricción | 23.0 °C | 40 % Show Material materials with Estricción of 40 % | |
Límite elástico Rp 0,2 | 23.0 °C | 415 MPa Show Material materials with Límite elástico Rp 0,2 of 415 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 585 MPa Show Material materials with Resistencia a la tracción of 585 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.05 - 0.1 % Show Material materials with Carbono of 0.05 - 0.1 % |
Cromo | 2.2 - 2.6 % Show Material materials with Cromo of 2.2 - 2.6 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.3 - 0.7 % Show Material materials with Manganeso of 0.3 - 0.7 % |
Molibdeno | 0.9 - 1.1 % Show Material materials with Molibdeno of 0.9 - 1.1 % |
Silicona | 0.15 - 0.45 % Show Material materials with Silicona of 0.15 - 0.45 % |
Titanio | 0.06 - 0.1 % Show Material materials with Titanio of 0.06 - 0.1 % |