General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.9 - 8.2 g/cm³ Show Material materials with Densidad of 7.9 - 8.2 g/cm³ | Typical for Austenitic Stainless Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Austenitic Stainless Steel |
Dureza Brinell | 23.0 °C | 192 [-] Show Material materials with Dureza Brinell of 192 [-] | |
Dureza Rockwell B | 23.0 °C | 90 [-] Show Material materials with Dureza Rockwell B of 90 [-] | |
Dureza Vickers | 23.0 °C | 200 [-] Show Material materials with Dureza Vickers of 200 [-] | |
Elongación A50 | 23.0 °C | 35 % Show Material materials with Elongación A50 of 35 % | |
Límite elástico | 23.0 °C | 230 MPa Show Material materials with Límite elástico of 230 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 23.0 °C | 195 GPa Show Material materials with Módulo elástico of 195 GPa | Typical for Austenitic Stainless Steel |
Resistencia a la tracción | 23.0 °C | 540 MPa Show Material materials with Resistencia a la tracción of 540 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 440 J/(kg·K) Show Material materials with Calor específico of 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.7E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 - 1.9E-5 1/K | Typical for Austenitic Stainless Steel |
Conductividad térmica | 23.0 °C | 11 - 21 W/(m·K) Show Material materials with Conductividad térmica of 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Temperatura de fusión | 1230 - 1480 °C Show Material materials with Temperatura de fusión of 1230 - 1480 °C | Typical for Austenitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.06 - 0.15 % Show Material materials with Carbono of 0.06 - 0.15 % |
Cromo | 14 - 16 % Show Material materials with Cromo of 14 - 16 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Manganeso | 5.5 - 7 % Show Material materials with Manganeso of 5.5 - 7 % |
Molibdeno | 0.8 - 1.2 % Show Material materials with Molibdeno of 0.8 - 1.2 % |
Niobio | 0.75 - 1.25 % Show Material materials with Niobio of 0.75 - 1.25 % |
Níquel | 9 - 11 % Show Material materials with Níquel of 9 - 11 % |
Silicona | 0.2 - 1 % Show Material materials with Silicona of 0.2 - 1 % |