General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 250 [-] Show Material materials with Dureza Brinell of 250 [-] | |
Dureza Rockwell C | 23.0 °C | 25 [-] Show Material materials with Dureza Rockwell C of 25 [-] | |
Dureza Vickers | 23.0 °C | 265 [-] Show Material materials with Dureza Vickers of 265 [-] | |
Elongación A50 | 23.0 °C | 20 % Show Material materials with Elongación A50 of 20 % | |
Límite elástico | 23.0 °C | 440 MPa Show Material materials with Límite elástico of 440 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 620 MPa Show Material materials with Resistencia a la tracción of 620 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Boro | 3E-4 - 6E-3 % Show Material materials with Boro of 3E-4 - 6E-3 % |
Carbono | 0.09 - 0.13 % Show Material materials with Carbono of 0.09 - 0.13 % |
Cromo | 8.5 - 9.5 % Show Material materials with Cromo of 8.5 - 9.5 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.3 - 0.6 % Show Material materials with Manganeso of 0.3 - 0.6 % |
Molibdeno | 0.9 - 1.1 % Show Material materials with Molibdeno of 0.9 - 1.1 % |
Niobio | 0.06 - 0.1 % Show Material materials with Niobio of 0.06 - 0.1 % |
Nitrógeno | 0.04 - 0.09 % Show Material materials with Nitrógeno of 0.04 - 0.09 % |
Níquel | 0.4 % Show Material materials with Níquel of 0.4 % |
Silicona | 0.1 - 0.5 % Show Material materials with Silicona of 0.1 - 0.5 % |
Vanadio | 0.18 - 0.25 % Show Material materials with Vanadio of 0.18 - 0.25 % |
Wolframio | 0.9 - 1.1 % Show Material materials with Wolframio of 0.9 - 1.1 % |