General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Dureza Brinell | 23.0 °C | 207 [-] Show Material materials with Dureza Brinell of 207 [-] | |
Dureza Rockwell B | 23.0 °C | 95 [-] Show Material materials with Dureza Rockwell B of 95 [-] | |
Elongación A50 | 23.0 °C | 20 % Show Material materials with Elongación A50 of 20 % | |
Límite elástico | 23.0 °C | 275 MPa Show Material materials with Límite elástico of 275 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 485 MPa Show Material materials with Resistencia a la tracción of 485 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % |
Cobre | 0.9 - 1.25 % Show Material materials with Cobre of 0.9 - 1.25 % |
Cromo | 18 - 23 % Show Material materials with Cromo of 18 - 23 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 0.75 % Show Material materials with Níquel of 0.75 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |