General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación A50 | 23.0 °C | 40 % Show Material materials with Elongación A50 of 40 % | |
Estricción | 23.0 °C | 50 % Show Material materials with Estricción of 50 % | |
Límite elástico Rp 0,2 | 23.0 °C | 205 MPa Show Material materials with Límite elástico Rp 0,2 of 205 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 23.0 °C | 515 MPa Show Material materials with Resistencia a la tracción of 515 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.15 % Show Material materials with Carbono of 0.15 % |
Cromo | 17 - 19 % Show Material materials with Cromo of 17 - 19 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Nitrógeno | 0.1 % Show Material materials with Nitrógeno of 0.1 % |
Níquel | 8 - 10 % Show Material materials with Níquel of 8 - 10 % |
Silicona | 2 - 3 % Show Material materials with Silicona of 2 - 3 % |