General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Chromium Molybdenum Steel | |||
Elongación | 18 % Show Material materials with Elongación of 18 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate | A200 |
19.2 % Show Material materials with Elongación of 19.2 % | Predicted Value, A80 | ||||
19.3 % Show Material materials with Elongación of 19.3 % | Predicted Value, Transverse | ||||
19.9 % Show Material materials with Elongación of 19.9 % | Predicted Value, A80 Transverse | ||||
22 % Show Material materials with Elongación of 22 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate | A50 | |
26.2 % Show Material materials with Elongación of 26.2 % | Predicted Value | ||||
Estricción | 43.8 % Show Material materials with Estricción of 43.8 % | Predicted Value, Transverse | |||
45.1 % Show Material materials with Estricción of 45.1 % | Predicted Value | ||||
Límite elástico | 230 MPa Show Material materials with Límite elástico of 230 MPa | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate | |
260.6 MPa Show Material materials with Límite elástico of 260.6 MPa | Predicted Value, RP1 | ||||
305.2 MPa Show Material materials with Límite elástico of 305.2 MPa | Predicted Value, RP05 | ||||
317.1 MPa Show Material materials with Límite elástico of 317.1 MPa | Predicted Value, RP1 Transverse | ||||
327 MPa Show Material materials with Límite elástico of 327 MPa | Predicted Value, Transverse | ||||
332.6 MPa Show Material materials with Límite elástico of 332.6 MPa | Predicted Value, RP02 | ||||
437.1 MPa Show Material materials with Límite elástico of 437.1 MPa | Predicted Value, RP002 | ||||
469.5 MPa Show Material materials with Límite elástico of 469.5 MPa | Predicted Value, RP02 Transverse | ||||
Módulo de cizallamiento | 79.3 GPa Show Material materials with Módulo de cizallamiento of 79.3 GPa | Predicted Value | |||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Chromium Molybdenum Steel | |||
Resistencia a la tracción | 380 - 550 MPa Show Material materials with Resistencia a la tracción of 380 - 550 MPa | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate | |
Resistencia al cizallamiento | 606.1 MPa Show Material materials with Resistencia al cizallamiento of 606.1 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 448 - 502 J/(kg·K) Show Material materials with Calor específico of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Coeficiente de dilatación térmica | 1.1e-05 - 1.4e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1e-05 - 1.4e-05 1/K | Typical for Chromium Molybdenum Steel |
Conductividad térmica | 36 - 43 W/(m·K) Show Material materials with Conductividad térmica of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Carbono | 0.05 - 0.17 % Show Material materials with Carbono of 0.05 - 0.17 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Cromo | 0.8 - 1.15 % Show Material materials with Cromo of 0.8 - 1.15 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Manganeso | 0.4 - 0.65 % Show Material materials with Manganeso of 0.4 - 0.65 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Molibdeno | 0.45 - 0.6 % Show Material materials with Molibdeno of 0.45 - 0.6 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |