Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 22 % Show Material materials with Elongación A50 of 22 % |
Elongation A200 | 20.0 °C | 18 % Show Material materials with Elongation A200 of 18 % |
Límite elástico | 20.0 °C | 230 MPa Show Material materials with Límite elástico of 230 MPa |
Resistencia a la tracción | 20.0 °C | 380 - 550 MPa Show Material materials with Resistencia a la tracción of 380 - 550 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.05 - 0.21 % Show Material materials with Carbono of 0.05 - 0.21 % |
Cromo | 0.5 - 0.8 % Show Material materials with Cromo of 0.5 - 0.8 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.55 - 0.8 % Show Material materials with Manganeso of 0.55 - 0.8 % |
Molibdeno | 0.45 - 0.6 % Show Material materials with Molibdeno of 0.45 - 0.6 % |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % |