General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel | |||
Elongación | 16.6 % Show Material materials with Elongación of 16.6 % | Predicted Value, A200 | |||
18 % Show Material materials with Elongación of 18 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate | A50 | |
18.8 % Show Material materials with Elongación of 18.8 % | Predicted Value, Transverse | ||||
20 % Show Material materials with Elongación of 20 % | Predicted Value, A80 Transverse | ||||
22.2 % Show Material materials with Elongación of 22.2 % | Predicted Value, A80 | ||||
25.9 % Show Material materials with Elongación of 25.9 % | Predicted Value | ||||
Estricción | 43.3 % Show Material materials with Estricción of 43.3 % | Predicted Value, Transverse | |||
45 % Show Material materials with Estricción of 45 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate | ||
Límite elástico | 205 MPa Show Material materials with Límite elástico of 205 MPa | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate | |
254.7 MPa Show Material materials with Límite elástico of 254.7 MPa | Predicted Value, RP1 | ||||
310.6 MPa Show Material materials with Límite elástico of 310.6 MPa | Predicted Value, Transverse | ||||
320.5 MPa Show Material materials with Límite elástico of 320.5 MPa | Predicted Value, RP1 Transverse | ||||
326.6 MPa Show Material materials with Límite elástico of 326.6 MPa | Predicted Value, RP05 | ||||
334.7 MPa Show Material materials with Límite elástico of 334.7 MPa | Predicted Value, RP02 | ||||
438 MPa Show Material materials with Límite elástico of 438 MPa | Predicted Value, RP02 Transverse | ||||
452.7 MPa Show Material materials with Límite elástico of 452.7 MPa | Predicted Value, RP002 | ||||
Módulo de cizallamiento | 79.3 GPa Show Material materials with Módulo de cizallamiento of 79.3 GPa | Predicted Value | |||
Módulo elástico | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel | |||
Resistencia a la tracción | 415 - 585 MPa Show Material materials with Resistencia a la tracción of 415 - 585 MPa | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate | |
Resistencia al cizallamiento | 628.2 MPa Show Material materials with Resistencia al cizallamiento of 628.2 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 458.9 J/(kg·K) Show Material materials with Calor específico of 458.9 J/(kg·K) | Predicted Value |
Coeficiente de dilatación térmica | 11.99 1/K Show Material materials with Coeficiente de dilatación térmica of 11.99 1/K | Predicted Value |
Conductividad térmica | 36.62 W/(m·K) Show Material materials with Conductividad térmica of 36.62 W/(m·K) | Predicted Value |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Carbono | 0.05 - 0.15 % Show Material materials with Carbono of 0.05 - 0.15 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Cromo | 2 - 2.5 % Show Material materials with Cromo of 2 - 2.5 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Manganeso | 0.3 - 0.6 % Show Material materials with Manganeso of 0.3 - 0.6 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Molibdeno | 0.9 - 1.1 % Show Material materials with Molibdeno of 0.9 - 1.1 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % | Class 1, Annealed, Normalized and Tempered, or Quenched and Tempered | ASTM A387 | Plate |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |