Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 0 - 18 % Show Material materials with Elongación A50 of 0 - 18 % |
Estricción | 20.0 °C | 0 - 45 % Show Material materials with Estricción of 0 - 45 % |
Límite elástico | 20.0 °C | 0 - 205 MPa Show Material materials with Límite elástico of 0 - 205 MPa |
Resistencia a la tracción | 20.0 °C | 415 - 585 MPa Show Material materials with Resistencia a la tracción of 415 - 585 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0 - 0.025 % Show Material materials with Azufre of 0 - 0.025 % |
Carbono | 0 - 0.15 % Show Material materials with Carbono of 0 - 0.15 % |
Cromo | 4 - 6 % Show Material materials with Cromo of 4 - 6 % |
Fósforo | 0 - 0.03 % Show Material materials with Fósforo of 0 - 0.03 % |
Manganeso | 0.3 - 0.6 % Show Material materials with Manganeso of 0.3 - 0.6 % |
Molibdeno | 0.45 - 0.65 % Show Material materials with Molibdeno of 0.45 - 0.65 % |
Silicona | 0 - 0.5 % Show Material materials with Silicona of 0 - 0.5 % |