Mecánica
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Carbono | 0.07 % Show Material materials with Carbono of 0.07 % |
Cromo | 19 - 21 % Show Material materials with Cromo of 19 - 21 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 2 - 3 % Show Material materials with Molibdeno of 2 - 3 % |
Níquel | 32 - 38 % Show Material materials with Níquel of 32 - 38 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |