Mecánica
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.04 % Show Material materials with Carbono of 0.04 % |
Cromo | 19 - 23 % Show Material materials with Cromo of 19 - 23 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Molibdeno | 4.3 - 5 % Show Material materials with Molibdeno of 4.3 - 5 % |
Níquel | 24 - 26 % Show Material materials with Níquel of 24 - 26 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |