Mecánica
Chemical properties
Property | Value |
---|---|
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.06 - 0.1 % Show Material materials with Carbono of 0.06 - 0.1 % |
Cromo | 19 - 23 % Show Material materials with Cromo of 19 - 23 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Níquel | 30 - 35 % Show Material materials with Níquel of 30 - 35 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Titanio | 0.15 - 0.6 % Show Material materials with Titanio of 0.15 - 0.6 % |