General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.7 - 8.7 g/cm³ Show Material materials with Densidad of 7.7 - 8.7 g/cm³ | Typical for Leaded Phosphor Bronze |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Dureza Brinell | 23.0 °C | 130 [-] Show Material materials with Dureza Brinell of 130 [-] | |
Dureza Rockwell B | 23.0 °C | 75 [-] Show Material materials with Dureza Rockwell B of 75 [-] | |
Elongación A50 | 23.0 °C | 10 % Show Material materials with Elongación A50 of 10 % | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Resistencia a la tracción | 23.0 °C | 415 MPa Show Material materials with Resistencia a la tracción of 415 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 380 J/(kg·K) Show Material materials with Calor específico of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Aluminio | 6 - 8 % Show Material materials with Aluminio of 6 - 8 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 1.5 - 3.5 % Show Material materials with Hierro of 1.5 - 3.5 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Plomo | 0.01 % Show Material materials with Plomo of 0.01 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |